Materials |
|
|---|---|
|
Main Components: |
Polysulfone (amber tint) |
|
O-rings: |
Silicone (clear), platinum-cured |
OPERATING CONDITIONS (FLUID TRANSFER) |
|
|---|---|
|
Pressure: |
Up to 35 psi, 2.41 bar |
|
Temperature: |
-40°F to 300°F (-40°C to 149°C) |
STERILIZATION |
|
|---|---|
|
Gamma: |
Up to 50kGy irradiation |
|
Autoclave: |
Up to 270°F (132°C) for 60 minutes, up to 25 repetitions. Sterilize uncoupled only. |
CV VALUE |
|---|
|
Cv~20.9 (301.14) max |
|
Cv values are based on gpm and psi, and Ipm and bar |