OPERATING CONDITIONS (FLUID TRANSFER) |
|
|---|---|
|
Pressure: |
Vacuum to 60 psi, 4.14 bar |
|
Temperature: |
Polycarbonate: -40°F to 250°F (-40°C to 121°C) |
|
Polysulfone: -40°F to 300°F (-40°C to 149°C) |
|
Sterilization |
|
|---|---|
|
Gamma irradiation: |
Up to 50 kGy irradiation |
|
Autoclave: |
Polycarbonate: Up to 250°F (121°C), 30 minutes, up to 10 repetitions. Sterilize uncoupled only. |
|
Polysulfone: Up to 270°F (132°C) for 60 minutes, up to 25 repetitions. Sterilize uncoupled only. |
|
MATERIALS |
|
|---|---|
|
Main component: |
Polycarbonate (purple tint) |
|
Polysulfone (amber tint) |
|
|
Locking Sleeves: |
Polysulfone (white) |
|
Thumb latches: |
Polycarbonate (white), PVDF (white) |
|
O-rings: |
Silicone (clear), platinum-cured; Buna-N (black) - (not USP Class VI or ADCF) |
OTHER |
|
|---|---|
|
Tubing sizes: |
1/8", 1/4" and 3/8" ID (3.22mm, 6.4mm and 9.5mm ID) |
CV VALUE |
|---|
|
Cv~5.5 (79.25) max |
|
Cv values are based on gpm and psi, and Ipm and bar (shown in parentheses). |
OPERATING CONDITIONS (FLUID TRANSFER) |
|
|---|---|
|
Pressure: |
Vacuum to 60 psi, 4.14 bar |
|
Temperature: |
Polycarbonate: -40°F to 250°F (-40°C to 121°C) |
|
Polysulfone: -40°F to 300°F (-40°C to 149°C) |
|
Sterilization |
|
|---|---|
|
Gamma irradiation: |
Up to 50 kGy irradiation |
|
Autoclave: |
Polycarbonate: Up to 250°F (121°C), 30 minutes, up to 10 repetitions. Sterilize uncoupled only. |
|
Polysulfone: Up to 270°F (132°C) for 60 minutes, up to 25 repetitions. Sterilize uncoupled only. |
|
MATERIALS |
|
|---|---|
|
Main component: |
Polycarbonate (purple tint) |
|
Polysulfone (amber tint) |
|
|
Locking Sleeves: |
Polysulfone (white) |
|
Thumb latches: |
Polycarbonate (white), PVDF (white) |
|
O-rings: |
Silicone (clear), platinum-cured; Buna-N (black) - (not USP Class VI or ADCF) |
OTHER |
|
|---|---|
|
Tubing sizes: |
1/8", 1/4" and 3/8" ID (3.22mm, 6.4mm and 9.5mm ID) |
CV VALUE |
|---|
|
Cv~5.5 (79.25) max |
|
Cv values are based on gpm and psi, and Ipm and bar (shown in parentheses). |
Loading